Due to errors in casting procedures, undesired irregularities or defects can be noticed. They can be observed as distortion which could be either in change in size or shape. Surface roughness or irregularities, porosities. It can be also be observed as incomplete or missing detail. Knowledge about t...
Due to errors in casting procedures, undesired irregularities or defects can be noticed. They can be observed as distortion which could be either in change in size or shape. Surface roughness or irregularities, porosities. It can be also be observed as incomplete or missing detail. Knowledge about the causes of distortion, would help in prevention of the same.